To evaluate if depth of cure D(ISO) determined by the ISO 4049 method is accurately reflected with bulk fill materials when compared to depth of cure D(new) determined by Vickers microhardness profiles. D(ISO) was determined according to "ISO 4049; Depth of cure" and resin composite specimens (n=6 per group) were prepared of two control materials (Filtek Supreme Plus, Filtek Silorane) and four bulk fill materials (Surefil SDR, Venus Bulk Fill, Quixfil, Tetric EvoCeram Bulk Fill) and light-cured for either 10s or 20s. For D(new), a mold was filled with one of the six resin composites and light-cured for either 10 s or 20 s (n=22 per group). The mold was placed under a microhardness indentation device and hardness measurements (Vickers hardness, VHN) were made at defined distances, beginning at the resin composite that had been closest to the light-curing unit (i.e. at the "top") and proceeding toward the uncured resin composite (i.e. toward the "bottom"). On the basis of the VHN measurements, Vickers hardness profiles were generated for each group. D(ISO) varied between 1.76 and 6.49 mm with the bulk fill materials showing the highest D(ISO). D(new) varied between 0.2 and 4.0 mm. D(new) was smaller than D(ISO) for all resin composites except Filtek Silorane. For bulk fill materials the ISO 4049 method overestimated depth of cure compared to depth of cure determined by Vickers hardness profiles. Copyright © 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Citation

Simon Flury, Stefanie Hayoz, Anne Peutzfeldt, Jürg Hüsler, Adrian Lussi. Depth of cure of resin composites: is the ISO 4049 method suitable for bulk fill materials? Dental materials : official publication of the Academy of Dental Materials. 2012 May;28(5):521-8

Expand section icon Mesh Tags

Expand section icon Substances


PMID: 22391146

View Full Text